鋁卷在鑄軋上會偶爾出現質量問題及時整改

來源:http://m.gbpeixun.com/ 發布時間:2022-05-07

  鋁卷是鑄軋機經過壓延,拉彎角加工后,為進行飛剪的金屬產品。廣泛應用在電子,包裝,建筑,機械等方面,那么鋁卷在鑄軋上會偶爾出現質量問題嗎?要怎么整改解決呢?
  Aluminum coil is cast rolling machine after calendering, bending processing, for flying shear metal products. Widely used in electronics, packaging, construction, machinery and other aspects, then aluminum coil in casting and rolling will occasionally have quality problems? How to rectify the solution?
  氣條和夾渣
  鋁卷在鑄軋上可能產生的原因:生產工藝沒嚴格執行(精煉不到位)、爐外除氣不到位(除氣箱漏氣)、鋁水處理不到位、過濾作用不明顯、空氣濕氣太重。整改措施:進行一次性投料、按操作工藝撒覆蓋劑、加強精煉、解決除氣箱漏氣問題、鋁水處理干凈、增加過濾裝置保證鋁水經過過濾。
  Air strip and slag
  The possible causes of aluminum coil in casting and rolling are as follows: the production process is not strictly implemented (refining is not in place), the gas removal outside the furnace is not in place (gas tank leakage), the aluminum water treatment is not in place, the filtration effect is not obvious, and the air moisture is too heavy. Rectification measures: one-time feeding, covering agent spreading according to the operation process, strengthening refining, solving the problem of air leakage in the degassing box, cleaning the aluminum water, adding filtration devices to ensure that the aluminum water is filtered.
  長條狀小裂口
  鋁卷鑄軋上可能產生的原因:咀皮損壞或損傷。整改措施:咀皮存在以上問題立刻斷板,保證生產時咀皮完好。
  Long striate small cleft
  Possible causes of aluminum roll casting: tip skin damage or damage. Corrective measures: if the above problems exist, the plates will be broken immediately to ensure that the plates are in good condition during production.


  黑條
  鋁卷鑄軋上可能存在的問題:工藝沒有執行到位,鋁水處理不好。整改措施:制定生產工藝,加強鋁水處理。
  Article black.
  Possible problems in aluminum roll casting: the process is not implemented in place, and the aluminum water treatment is not good. Corrective measures: develop production process, strengthen aluminum water treatment.
  擦劃傷
  鋁卷鑄軋可能產生的原因:剪板機下臺面磨擦鋁板表面造成。整改措施:對剪板機下臺面進行整改。
  Clean cut
  Aluminum roll casting and rolling may be caused by the friction of the surface of the plate shearing machine. Rectification measures: rectification of the shearing machine stepping down surface.
  鋁卷具有密度低,使用壽命比較長,外表漂亮美觀的特征,是電廠、化工廠管道保溫不可缺少的產品。鋁卷生產廠家提醒,為了更好的使用鋁卷,延長鋁卷的使用壽命,那么對鋁卷的儲存環境也有比較嚴格的要求。
  Aluminum coil has the characteristics of low density, long service life and beautiful appearance. It is an indispensable product for pipeline insulation in power plants and chemical plants. Aluminum coil manufacturers remind, in order to better use aluminum coil, prolong the service life of aluminum coil, then the storage environment of aluminum coil also have more strict requirements.
  要確保存放的環境要通風,干燥千萬不要放到潮濕的地方,鋁卷屬于有色金屬如果與水觸摸以后會發作氧化反應,這樣鋁卷表面就會損壞掉,外表會形成一種保護膜,確切的話會形成一片一片的白色氧化痕跡,致使外觀量受到影響,所以一個干燥的環境是存放鋁卷的必要條件。
  To ensure storage environment to ventilation, dry places, don't put wet aluminum volume belongs to non-ferrous metal if touch will attack oxidation reaction with water, this will damage off aluminum roll surface, appearance can form a protective film, the exact words will form a piece of white oxidation, the appearance of affected, So a dry environment is a necessary condition for the storage of aluminum coils.
  鋁卷很多地方也有生產,但是大家在購買的時候,千萬不能馬虎大意,可以多加對比,這樣才能選擇到物美價廉的鋁卷。更多問題的了解大家可以來網站m.gbpeixun.com進行相應的咨詢。
  Aluminum coil is also produced in many places, but when we buy, do not be careless, can be more contrast, so as to choose inexpensive aluminum coil. For more information, please visit m.gbpeixun.com for consultation.